您的位置: 专家智库 > >

国家重点基础研究发展计划(2010CB30806)

作品数:2 被引量:30H指数:2
相关作者:曾智邓小旋魏鹏远王新华李林平更多>>
相关机构:首钢集团北京科技大学更多>>
发文基金:国家重点基础研究发展计划更多>>
相关领域:冶金工程更多>>

文献类型

  • 2篇中文期刊文章

领域

  • 2篇冶金工程

主题

  • 1篇铸坯
  • 1篇连铸
  • 1篇连铸板坯
  • 1篇帘线钢
  • 1篇炉渣
  • 1篇炉渣碱度
  • 1篇洁净度
  • 1篇碱度
  • 1篇工业应用试验
  • 1篇钢包
  • 1篇板坯
  • 1篇DESULF...
  • 1篇IF钢
  • 1篇MGO含量
  • 1篇BASICI...

机构

  • 1篇北京科技大学
  • 1篇首钢集团

作者

  • 1篇季晨曦
  • 1篇李林平
  • 1篇王新华
  • 1篇魏鹏远
  • 1篇邓小旋
  • 1篇曾智

传媒

  • 1篇北京科技大学...
  • 1篇Journa...

年份

  • 1篇2014
  • 1篇2013
2 条 记 录,以下是 1-2
排序方式:
Industrial Application of Desulfurization Using Low Basicity Refining Slag in Tire Cord Steel被引量:12
2013年
Desulfurization performance with low binary basicity refining slag in 72 grade tire cord steel was calculated using FactSage and it is found that sulfur content in steel decreases with the increase of basicity of slag, MgO content in slag and slag/steel ratio while sulfur partition ratio between slag and steel increases gradually with the increase of basicity of slag as well as MgO content. Experiments were carried out and the results are of great agreements with theoretical calculation. Then industrial application tests were performed in a domestic plant and good results were achieved. Sulfur content in steel decreases gradually during refining process, as a result, sulfur content in the billets is controlled in the range of 0.007 1%-0.008 1%. Sulfur content in steel refined with slag basicity of 1.21 is lower than that of 1.02, while the plasticity of oxide compound inclusions is a little better controlled in low basicity heats. Using refining slag with basicity of 1.0-1.2 and MgO content of 5%-10% and reducing the slag takeover of LD are favorable for improving the desulfurization performance and the plasticity of inclusions during the industrial production.
CHEN Shu-haoWANG Xin-huaHE Xiao-feiWANG Wan-junJIANG Min
关键词:工业应用试验帘线钢MGO含量炉渣碱度
交换钢包过程对IF钢连铸板坯表层洁净度的影响被引量:18
2014年
采用ASPEX扫描电镜中的自动特征分析功能研究了交换钢包过程(取样浇次第4、5炉)对IF钢连铸板坯表层的洁净度的影响,且对比研究了交换钢包过程浇铸铸坯(交接坯)与正常浇铸铸坯(正常坯)的表层洁净度.结果表明:正常坯与交接坯中尺寸大于20μm的表层夹杂物可分为三类:(1)簇群状Al2O3(包括气泡+簇群状Al2O3);(2)簇群状TiOx--Al2O3夹杂物;(3)保护渣夹杂物.正常坯表层的大型夹杂物主要为簇群状Al2O3,没有检测到保护渣夹杂物.换包开浇后铸坯总氧质量分数从14×10-6增至17×10-6,交接坯表层检测到较多的第2夹杂物,说明钢包开浇后钢水被轻微氧化.此外,钢包开浇后剧烈的液面波动也导致了保护渣的卷入.在当前工艺下,换包对IF钢铸坯表层洁净度的影响长度约为11m.
邓小旋王新华李林平魏鹏远季晨曦曾智田志红
关键词:IF钢连铸铸坯洁净度