Aragonite calcium carbonate whisker was prepared by thermal decomposition of Ca(HCO3)2 in aqueous solution in the presence of chloride salts. The influences of reaction temperature, time and concentrations of CaCl2, MgCl2 and KCl on the morphology of CaCO3 whiskers were studied. The structure characteristics of CaCO3 whiskers were analyzed by XRD and SEM. The results indicate that the optimum conditions are 80~100 ℃, 50~60 min and the suitable concentrations of Ca(HCO3)2, KCl, MgCl2, CaCl2 are 6.0 mmol/L, 14.0 mmol/L, 1.0 mmol/L, 1.5 mmol/L respectively. The purity of the whiskers is 99.53% and the average aspect ratio is 24.1.
以明胶为反应介质,采用凝胶网格控制合成法制备了单分散球形纳米ZnO光催化剂.利用TG-DTA、XRD、TEM、BET、UV-Vis、HPLC等测试手段对制备过程、样品的结构和性能进行了研究,探讨了明胶浓度、煅烧温度对产物粒径和光催化活性的影响.结果表明:利用凝胶网格控制合成法不仅能够控制纳米微粒的形状和大小,而且可防止沉淀物相互聚集和团聚.以染料罗丹明B溶液为目标降解物,1 h的降解率为99.9%,最佳光催化剂的合成条件:13%明胶浓度、350℃煅烧2 h.